详情
KL-918B3
Type of coating: Iron powder low hydrogen type
KL-918B3 is suitable for welding Cr-Mo alloy steel
Classification
.png)
Application and Features
- KL-918B3 is suitable for welding Cr-Mo alloy steel
- It provides high deposition rate and good weldability
- Weld metal contains 2.25%Cr-1%Mo,such as ASTM A387Gr.22 and JIS SCMV4
- It is ideal for welding high pressure steel pipes, heat exchanger steel pipes of boilers and steels for petro-chemical plants
Welding Position
Welding Instruction
- Clean up the contaminations on the steel.
- Dry the electrodes at 350~400°C for 60 minutes before welding.
- Keep arc as short as possible. Take the back step method to prevent porosity at arc start and re-start. (Please refer to Appendix A)
- Preheat and interpass temperature: 160~190°C, PWHT: 675~705°C
Application
- KL-916B3 is suitable for welding Cr-Mo alloy steel
Typical Chemical Composition of Weld Metal (wt%)
Typical Mechanical Properties of Weld Metal
Size and Suggested Operation Range (AC or DC±)