							Tensile Strength | 
							Elongation at Break | 
							Maximum 
							Abrasion Loss | 
							Polymer Rubber | 
							Working Temperature | |
| 
							mpa | 
							% min | 
							Mm3 | 
							Degree Centigrade | ||
| 
							OR | 
							15 | 
							300% | 
							150 | 
							NBR Blended | 
							-30 to +60 | 
| 
							MOR | 
							12 | 
							300% | 
							300 | 
							NBR Blended | 
							-30 to +50 | 
| 
							OHR | 
							15 | 
							400% | 
							180 | 
							NBR Blended | 
							+ 100 lump | 
 Malaysia